Laboratory Crucibles Cylindrical Shape (Z)
Spinel (SP-30‑G)
70% Al2O3 30% MgO
Model | Øout | Height | Wall | Vol | Request |
---|---|---|---|---|---|
Z 15 | 15 | 20 | 2 | 2 | |
Z 20 | 20 | 24 | 2 | 3 | |
Z 25 | 25 | 50 | 2 | 15 | |
Z 30 | 30 | 39 | 2 | 15 | |
Z 32 | 33 | 76 | 2 | 40 | |
Z 38 | 38 | 43 | 2 | 25 | |
Z 39 | 39 | 100 | 2 | 90 | |
Z 40 | 40 | 54 | 2 | 40 | |
Z 40/1 | 40 | 79 | 3 | 70 | |
Z 43 | 44 | 85 | 3 | 90 | |
Z 44 | 44 | 51 | 3 | 50 | |
Z 46 | 46 | 54 | 3 | 60 | |
Z 50 | 50 | 69 | 3 | 90 | |
Z 51 | 52 | 39 | 3 | 50 | |
Z 52 | 54 | 30 | 3 | 35 | |
Z 56 | 57 | 85 | 3 | 140 | |
Z 58 | 58 | 62 | 3 | 100 | |
Z 60 | 60 | 84 | 3 | 170 | |
Z 60/1 | 57 | 60 | 4 | 110 | |
Z 64 | 65 | 130 | 4 | 300 | |
Z 65 | 65 | 70 | 3 | 195 | |
Z 70 | 69 | 98 | 3 | 260 | |
Z 80 | 77 | 113 | 4 | 420 | |
Z 80/1 | 81 | 152 | 4 | 560 | |
Z 90 | 90 | 129 | 4–5 | 600 | |
Z 100 | 100 | 144 | 4 — 5 | 900 | |
Z 105 | 104 | 156 | 4 — 5 | 1000 | |
Z 115 | 118 | 178 | 4 — 5 | 1500 | |
Z 115/1 | 118 | 114 | 4 — 5 | 900 | |
Z 130 | 128 | 147 | 4 — 5 | 1500 | |
Z 115/2 | 118 | 214 | 4 — 5 | 1800 |
Legend
Øout | Outside diameter in mm |
Height | Height in mm |
Wall | Wall thickness in mm |
Vol | Volume in ml |
SPECIAL PROPERTIES
- good thermal and chemical resistance to aggressive alkalis
- high thermal conductivity
- comparatively good thermal shock resistance
- Good to very good chemical resistance to: lead, manganese, hydrochloric acid (30%), silver
Directional Analysis
Cast Spinel (dense)
Quality SP-30‑G